Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   France. Stainless steel    

Equivalents to grade Z5CN18-11FF

    Country   -   France         Standard   -   AFNOR NF         Grade   -   Z5CN18-11FF    

    06KH18N11   ( 06Х18Н11 )   -   Corrosion-resistant steel for general purposes

  06KH18N11   ( 06Х18Н11 ),      

06KH18N11   ( 06Х18Н11 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties


Z5CN18-11FF France Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com