Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - USA | Standard - SAE | Grade - 3120 |
20KHN ( 20ХН ) - Alloy structurall steel 20KH2N4А ( 20Х2Н4А ) - Alloy structurall steel 20KHN ( 20ХН ), 20KH2N4А ( 20Х2Н4А ), |
- |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |