Equivalents to grade 42Cr4

    Country   -   Spain         Standard   -   UNE         Grade   -   42Cr4    

    40KH   ( 40Х )   -   Alloy structurall steel

  40KH   ( 40Х ),      

40KH   ( 40Х )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 40KH   ( 40Х )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire


42Cr4 Spain Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru