    Country   -   Italy         Standard   -   UNI 7070         Grade   -   Fe510D    

    17GS ( 17ГС )   -   Low alloy structural steel for welding construct
    17G1S ( 17Г1С )   -   Low alloy structural steel for welding construct

  17GS ( 17ГС ),         17G1S ( 17Г1С ),      