Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - England | Standard - BS EN 10083-1 | Grade - 28Mn6 |
30G ( 30Г ) - Alloy structurall steel 30G ( 30Г ), |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |