Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - Poland | Standard - PN/H 85020 | Grade - N13E |
U13А ( У13А ) - Carbon tool steel U13А ( У13А ), |
В32 - Graded and shaped rolling |