Country - Hungary | Standard - MSZ 21053 | Grade - AoX10CrNiMoTi18-12 |
12KH18N12M3TL ( 12Х18Н12М3ТЛ ) - Casting alloy steel with specific properties 12KH18N12M3TL ( 12Х18Н12М3ТЛ ), |
B82 - Steel Castings |