Ferro-alloys - all grades


Metallic manganese and nitrated manganese
      Mn87N6   ( Мн87Н6 )
      Mn89N4   ( Мн89Н4 )
      Mn91N2   ( Мн91Н2 )
      Mn92N6   ( Мн92Н6 )
      Mn95   ( Мн95 )
      Mn965   ( Мн965 )
      Mn997   ( Мн997 )
      Mn998   ( Мн998 )

Silico-calcium
      SK10   ( СК10 )
      SK10R   ( СК10Р )
      SK15   ( СК15 )
      SK15R   ( СК15Р )
      SK20   ( СК20 )
      SK20R   ( СК20Р )
      SK25   ( СК25 )
      SK25(Ch)   ( СК25(ч) )
      SK25R   ( СК25Р )
      SK30   ( СК30 )
      SK30(Ch)   ( СК30(ч) )
      SK30R   ( СК30Р )

Metal chrome
      ACr98   ( ACr98 )
      ACr98.5   ( ACr98.5 )
      ECr99.2   ( ECr99.2 )
      RACr99   ( RACr99 )
      RECr99.6   ( RECr99.6 )
      Kh97.5   ( Х97.5 )
      Kh98.5   ( Х98.5 )
      Kh99   ( Х99 )
      Kh99N1   ( Х99Н1 )
      Kh99N2   ( Х99Н2 )
      Kh99N4   ( Х99Н4 )
      Kh99N6   ( Х99Н5 )

Ferroboron
      FB12   ( ФБ12 )
      FB17   ( ФБ17 )
      FB20   ( ФБ20 )
      FB6   ( ФБ6 )

Ferrovanadium
      FeV40   ( FeV40 )
      FeV60   ( FeV60 )
      FeV80   ( FeV80 )
      FeV80A112   ( FeV80A112 )
      FeV80A114   ( FeV80A114 )
      FVd40U0.5   ( ФВд40У0.5 )
      FVd40U0.75   ( ФВд40У0.75 )
      FVd40U1   ( ФВд40У1 )
      FVd50U0.3   ( ФВд50У0.3 )
      FVd50U0.4   ( ФВд50У0.4 )
      FVd50U0.5   ( ФВд50У0.5 )
      FVd50U0.6   ( ФВд50У0.6 )
      FVd50U0.75   ( ФВд50У0.75 )
 

Ferrotungsten
      FeW80   ( FeW80 )
      FeW80LC   ( FeW80LC )
      FV65   ( ФВ65 )
      FV70   ( ФВ70 )
      FV70(a)   ( ФВ70(а) )
      FV72   ( ФВ72 )
      FV75(a)   ( ФВ75(а) )
      FV80(a)   ( ФВ80(а) )

Ferromanganese
      FeMn70C05N5   ( FeMn70C05N5 )
      FeMn70C05N5LP   ( FeMn70C05N5LP )
      FeMn70C10N5   ( FeMn70C10N5 )
      FeMn70C10N5LP   ( FeMn70C10N5LP )
      FeMn75C80HP   ( FeMn75C80HP )
      FeMn75C80LP   ( FeMn75C80LP )
      FeMn75C80MP   ( FeMn75C80MP )
      FeMn75C80VHP   ( FeMn75C80VHP )
      FeMn75C80VLP   ( FeMn75C80VLP )
      FeMn80C01   ( FeMn80C01 )
      FeMn80C01LP   ( FeMn80C01LP )
      FeMn80C05   ( FeMn80C05 )
      FeMn80C05LP   ( FeMn80C05LP )
      FeMn80C05N2   ( FeMn80C05N2 )
      FeMn80C10   ( FeMn80C10 )
      FeMn80C10LP   ( FeMn80C10LP )
      FeMn80C15   ( FeMn80C15 )
      FeMn80C15LP   ( FeMn80C15LP )
      FeMn80C20   ( FeMn80C20 )
      FeMn80C20LP   ( FeMn80C20LP )
      FeMn90C01   ( FeMn90C01 )
      FeMn90C01LP   ( FeMn90C01LP )
      FeMn90C05   ( FeMn90C05 )
      FeMn90C05LP   ( FeMn90C05LP )
      FeMn90C10   ( FeMn90C10 )
      FeMn90C10LP   ( FeMn90C10LP )
      FeMn90C15   ( FeMn90C15 )
      FeMn90C15LP   ( FeMn90C15LP )
      FeMn90C20   ( FeMn90C20 )
      FeMn90C20LP   ( FeMn90C20LP )
      FMn70(A)   ( ФМн70(А) )
      FMn70(B)   ( ФМн70(Б) )
      FMn78(A)   ( ФМн78(А) )
      FMn78(B)   ( ФМн78(Б) )
      FMn88(A)   ( ФМн88(А) )
      FMn88(B)   ( ФМн88(Б) )
      FMn90(A)   ( ФМн90(А) )
      FMn90(B)   ( ФМн90(Б) )

Ferromolybdenum
      FeMo60   ( FeMo60 )
      FeMo60Cu1   ( FeMo60Cu1 )
      FeMo60Cu1.5   ( FeMo60Cu1.5 )
      FeMo70   ( FeMo70 )
      FeMo70Cu1   ( FeMo70Cu1 )
      FeMo70Cu1.5   ( FeMo70Cu1.5 )
      FMo50   ( ФМо50 )
      FMo55   ( ФМо55 )
      FMo58   ( ФМо58 )
      FMo58(nk)   ( ФМо58(нк) )
      FMo60   ( ФМо60 )
      FMo60(nk)   ( ФМо60(нк) )

Ferroniobium
      FeNb60Ta1A13   ( FeNb60Ta1A13 )
      FeNb60Ta1A13.5   ( FeNb60Ta1A13.5 )
      FeNb60Ta1A16   ( FeNb60Ta1A16 )
      FeNb60Ta5A12   ( FeNb60Ta5A12 )
      FeNb60Ta5A16   ( FeNb60Ta5A16 )
      FeNb60Ta5A16Sn   ( FeNb60Ta5A16Sn )
      FeNb65   ( FeNb65 )
      FN650S   ( ФН650С )
      FN655(f)   ( ФН655(ф) )
      FN655S   ( ФН655С )
      FN658   ( ФН658 )
      FN658(f)   ( ФН658(ф) )
      FN660   ( ФН660 )
 

Ferrosilicium
      FeSi10   ( FeSi10 )
      FeSi15   ( FeSi15 )
      FeSi25   ( FeSi25 )
      FeSi45   ( FeSi45 )
      FeSi50   ( FeSi50 )
      FeSi65   ( FeSi65 )
      FeSi75Al1   ( FeSi75Al1 )
      FeSi75Al1.5   ( FeSi75Al1.5 )
      FeSi75Al2   ( FeSi75Al2 )
      FeSi75Al3   ( FeSi75Al3 )
      FeSi90Al1   ( FeSi90Al1 )
      FeSi90Al2   ( FeSi90Al2 )
      FS20   ( ФС20 )
      FS25   ( ФС25 )
      FS45   ( ФС45 )
      FS50   ( ФС50 )
      FS65   ( ФС65 )
      FS70   ( ФС70 )
      FS70Al1   ( ФС70Al1 )
      FS75   ( ФС75 )
      FS90   ( ФС90 )
 

Ferrosilicomanganese
      FeMnSi12   ( FeMnSi12 )
      FeMnSi18   ( FeMnSi18 )
      FeMnSi18LP   ( FeMnSi18LP )
      FeMnSi22HP   ( FeMnSi22HP )
      FeMnSi22LP   ( FeMnSi22LP )
      FeMnSi22MP   ( FeMnSi22MP )
      FeMnSi23HP   ( FeMnSi23HP )
      FeMnSi23LP   ( FeMnSi23LP )
      FeMnSi23MP   ( FeMnSi23MP )
      FeMnSi28   ( FeMnSi28 )
      FeMnSi28LP   ( FeMnSi28LP )
      FeMnSi30ELP   ( FeMnSi30ELP )
      FeMnSi30HP   ( FeMnSi30HP )
      FeMnSi30LP   ( FeMnSi30LP )
      MnS12(A)   ( МнС12(А) )
      MnS12(B)   ( МнС12(Б) )
      MnS17(A)   ( МнС17(А) )
      MnS17(B)   ( МнС17(Б) )
      MnS22(A)   ( МнС22(А) )
      MnS22(B)   ( МнС22(Б) )
      MnS25(A)   ( МнС25(А) )
      MnS25(B)   ( МнС25(Б) )

Ferrosilicochromium
      FeCrSi15   ( FeCrSi15 )
      FeCrSi22   ( FeCrSi22 )
      FeCrSi23   ( FeCrSi23 )
      FeCrSi26   ( FeCrSi26 )
      FeCrSi33   ( FeCrSi33 )
      FeCrSi40   ( FeCrSi40 )
      FeCrSi45   ( FeCrSi45 )
      FeCrSi48   ( FeCrSi48 )
      FeCrSi48LP   ( FeCrSi48LP )
      FeCrSi50   ( FeCrSi50 )
      FeCrSi50LC   ( FeCrSi50LC )
      FeCrSi55   ( FeCrSi55 )
      FKhS20   ( ФХС20 )
      FKhS20R   ( ФХС20Р )
      FKhS33   ( ФХС33 )
      FKhS33R   ( ФХС33Р )
      FKhS40   ( ФХС40 )
      FKhS40R   ( ФХС40Р )
      FKhS48   ( ФХС48 )
      FKhS48R   ( ФХС48Р )

Ferrotitanium
      FeT30A110   ( FeT30A110 )
      FeT30A16   ( FeT30A16 )
      FeT40A10   ( FeT40A10 )
      FeT40A16   ( FeT40A16 )
      FeT40A18   ( FeT40A18 )
      FeT70   ( FeT70 )
      FeT70A112   ( FeT70A112 )
      FeT70A15   ( FeT70A15 )
      FTi25   ( ФТи25 )
      FTi30   ( ФТи30 )
      FTi35S5   ( ФТи35С5 )
      FTi35S7   ( ФТи35С7 )
      FTi35S8   ( ФТи35С8 )
      FTi70S05   ( ФТи70С05 )
      FTi70S05Sn03   ( ФТи70С05Сн03 )
      FTi70S08   ( ФТи70С08 )
      FTi70S1   ( ФТи70С1 )
 

Ferrochromium
      FeCr50C01   ( FeCr50C01 )
      FeCr50C01LP   ( FeCr50C01LP )
      FeCr50C03   ( FeCr50C03 )
      FeCr50C03LP   ( FeCr50C03LP )
      FeCr50C05   ( FeCr50C05 )
      FeCr50C05LP   ( FeCr50C05LP )
      FeCr50C1   ( FeCr50C1 )
      FeCr50C10   ( FeCr50C10 )
      FeCr50C10LP   ( FeCr50C10LP )
      FeCr50C1LP   ( FeCr50C1LP )
      FeCr50C1N3   ( FeCr50C1N3 )
      FeCr50C1N7   ( FeCr50C1N7 )
      FeCr50C1N7Si   ( FeCr50C1N7Si )
      FeCr50C2   ( FeCr50C2 )
      FeCr50C20   ( FeCr50C20 )
      FeCr50C20LP   ( FeCr50C20LP )
      FeCr50C2LP   ( FeCr50C2LP )
      FeCr50C40   ( FeCr50C40 )
      FeCr50C40LP   ( FeCr50C40LP )
      FeCr50C5   ( FeCr50C5 )
      FeCr50C50   ( FeCr50C50 )
      FeCr50C50LP   ( FeCr50C50LP )
      FeCr50C50LS   ( FeCr50C50LS )
      FeCr50C50LSLP   ( FeCr50C50LSLP )
      FeCr50C50Si2   ( FeCr50C50Si2 )
      FeCr50C50Si2LP   ( FeCr50C50Si2LP )
      FeCr50C50Si2LS   ( FeCr50C50Si2LS )
      FeCr50C50Si2LSLP   ( FeCr50C50Si2LSLP )
      FeCr50C50Si4   ( FeCr50C50Si4 )
      FeCr50C50Si4LP   ( FeCr50C50Si4LP )
      FeCr50C50Si4LS   ( FeCr50C50Si4LS )
      FeCr50C50Si4LSLP   ( FeCr50C50Si4LSLP )
      FeCr50C50Si7   ( FeCr50C50Si7 )
      FeCr50C50Si7LP   ( FeCr50C50Si7LP )
      FeCr50C5LP   ( FeCr50C5LP )
      FeCr50C70   ( FeCr50C70 )
      FeCr50C70LP   ( FeCr50C70LP )
      FeCr50C70LS   ( FeCr50C70LS )
      FeCr50C70LSLP   ( FeCr50C70LSLP )
      FeCr50C70Si2   ( FeCr50C70Si2 )
      FeCr50C70Si2LP   ( FeCr50C70Si2LP )
      FeCr50C70Si2LS   ( FeCr50C70Si2LS )
      FeCr50C70Si2LSLP   ( FeCr50C70Si2LSLP )
      FeCr50C70Si4   ( FeCr50C70Si4 )
      FeCr50C70Si4LP   ( FeCr50C70Si4LP )
      FeCr50C70Si4LS   ( FeCr50C70Si4LS )
      FeCr50C70Si4LSLP   ( FeCr50C70Si4LSLP )
      FeCr50C70Si6   ( FeCr50C70Si6 )
      FeCr50C70Si6LP   ( FeCr50C70Si6LP )
      FeCr50C90   ( FeCr50C90 )
      FeCr50C90LP   ( FeCr50C90LP )
      FeCr50C90LS   ( FeCr50C90LS )
      FeCr50C90LSLP   ( FeCr50C90LSLP )
      FeCr50C90Si2   ( FeCr50C90Si2 )
      FeCr50C90Si2LP   ( FeCr50C90Si2LP )
      FeCr50C90Si2LS   ( FeCr50C90Si2LS )
      FeCr50C90Si2LSLP   ( FeCr50C90Si2LSLP )
      FeCr50C90Si4   ( FeCr50C90Si4 )
      FeCr50C90Si4LP   ( FeCr50C90Si4LP )
      FeCr50C90Si4LS   ( FeCr50C90Si4LS )
      FeCr50C90Si4LSLP   ( FeCr50C90Si4LSLP )
      FeCr60C01   ( FeCr60C01 )
      FeCr60C01LP   ( FeCr60C01LP )
      FeCr60C03   ( FeCr60C03 )
      FeCr60C03LP   ( FeCr60C03LP )
      FeCr60C05   ( FeCr60C05 )
      FeCr60C05LP   ( FeCr60C05LP )
      FeCr60C1   ( FeCr60C1 )
      FeCr60C10   ( FeCr60C10 )
      FeCr60C10LP   ( FeCr60C10LP )
      FeCr60C1LP   ( FeCr60C1LP )
      FeCr60C1N3   ( FeCr60C1N3 )
      FeCr60C1N7   ( FeCr60C1N7 )
      FeCr60C1N7Si   ( FeCr60C1N7Si )
      FeCr60C2   ( FeCr60C2 )
      FeCr60C20   ( FeCr60C20 )
      FeCr60C20LP   ( FeCr60C20LP )
      FeCr60C2LP   ( FeCr60C2LP )
      FeCr60C40   ( FeCr60C40 )
      FeCr60C40LP   ( FeCr60C40LP )
      FeCr60C5   ( FeCr60C5 )
      FeCr60C50   ( FeCr60C50 )
      FeCr60C50LP   ( FeCr60C50LP )
      FeCr60C50LS   ( FeCr60C50LS )
      FeCr60C50LSLP   ( FeCr60C50LSLP )
      FeCr60C50Si2   ( FeCr60C50Si2 )
      FeCr60C50Si2LP   ( FeCr60C50Si2LP )
      FeCr60C50Si2LS   ( FeCr60C50Si2LS )
      FeCr60C50Si2LSLP   ( FeCr60C50Si2LSLP )
      FeCr60C50Si4   ( FeCr60C50Si4 )
      FeCr60C50Si4LP   ( FeCr60C50Si4LP )
      FeCr60C50Si4LS   ( FeCr60C50Si4LS )
      FeCr60C50Si4LSLP   ( FeCr60C50Si4LSLP )
      FeCr60C50Si7   ( FeCr60C50Si7 )
      FeCr60C50Si7LP   ( FeCr60C50Si7LP )
      FeCr60C5LP   ( FeCr60C5LP )
      FeCr60C70   ( FeCr60C70 )
      FeCr60C70LP   ( FeCr60C70LP )
      FeCr60C70LS   ( FeCr60C70LS )
      FeCr60C70LSLP   ( FeCr60C70LSLP )
      FeCr60C70Si2   ( FeCr60C70Si2 )
      FeCr60C70Si2LP   ( FeCr60C70Si2LP )
      FeCr60C70Si2LS   ( FeCr60C70Si2LS )
      FeCr60C70Si2LSLP   ( FeCr60C70Si2LSLP )
      FeCr60C70Si4   ( FeCr60C70Si4 )
      FeCr60C70Si4LP   ( FeCr60C70Si4LP )
      FeCr60C70Si4LS   ( FeCr60C70Si4LS )
      FeCr60C70Si4LSLP   ( FeCr60C70Si4LSLP )
      FeCr60C70Si6   ( FeCr60C70Si6 )
      FeCr60C70Si6LP   ( FeCr60C70Si6LP )
      FeCr60C90   ( FeCr60C90 )
      FeCr60C90LP   ( FeCr60C90LP )
      FeCr60C90LS   ( FeCr60C90LS )
      FeCr60C90LSLP   ( FeCr60C90LSLP )
      FeCr60C90Si2   ( FeCr60C90Si2 )
      FeCr60C90Si2LP   ( FeCr60C90Si2LP )
      FeCr60C90Si2LS   ( FeCr60C90Si2LS )
      FeCr60C90Si2LSLP   ( FeCr60C90Si2LSLP )
      FeCr60C90Si4   ( FeCr60C90Si4 )
      FeCr60C90Si4LP   ( FeCr60C90Si4LP )
      FeCr60C90Si4LS   ( FeCr60C90Si4LS )
      FeCr60C90Si4LSLP   ( FeCr60C90Si4LSLP )
      FeCr70C01   ( FeCr70C01 )
      FeCr70C01LP   ( FeCr70C01LP )
      FeCr70C03   ( FeCr70C03 )
      FeCr70C03LP   ( FeCr70C03LP )
      FeCr70C05   ( FeCr70C05 )
      FeCr70C05LP   ( FeCr70C05LP )
      FeCr70C1   ( FeCr70C1 )
      FeCr70C10   ( FeCr70C10 )
      FeCr70C10LP   ( FeCr70C10LP )
      FeCr70C1LP   ( FeCr70C1LP )
      FeCr70C1N3   ( FeCr70C1N3 )
      FeCr70C1N7   ( FeCr70C1N7 )
      FeCr70C1N7Si   ( FeCr70C1N7Si )
      FeCr70C2   ( FeCr70C2 )
      FeCr70C20   ( FeCr70C20 )
      FeCr70C20LP   ( FeCr70C20LP )
      FeCr70C2LP   ( FeCr70C2LP )
      FeCr70C40   ( FeCr70C40 )
      FeCr70C40LP   ( FeCr70C40LP )
      FeCr70C5   ( FeCr70C5 )
      FeCr70C50   ( FeCr70C50 )
      FeCr70C50LP   ( FeCr70C50LP )
      FeCr70C50LS   ( FeCr70C50LS )
      FeCr70C50LSLP   ( FeCr70C50LSLP )
      FeCr70C50Si2   ( FeCr70C50Si2 )
      FeCr70C50Si2LP   ( FeCr70C50Si2LP )
      FeCr70C50Si2LS   ( FeCr70C50Si2LS )
      FeCr70C50Si2LSLP   ( FeCr70C50Si2LSLP )
      FeCr70C50Si4   ( FeCr70C50Si4 )
      FeCr70C50Si4LP   ( FeCr70C50Si4LP )
      FeCr70C50Si4LS   ( FeCr70C50Si4LS )
      FeCr70C50Si4LSLP   ( FeCr70C50Si4LSLP )
      FeCr70C50Si7   ( FeCr70C50Si7 )
      FeCr70C50Si7LP   ( FeCr70C50Si7LP )
      FeCr70C5LP   ( FeCr70C5LP )
      FeCr70C70   ( FeCr70C70 )
      FeCr70C70LP   ( FeCr70C70LP )
      FeCr70C70LS   ( FeCr70C70LS )
      FeCr70C70LSLP   ( FeCr70C70LSLP )
      FeCr70C70Si2   ( FeCr70C70Si2 )
      FeCr70C70Si2LP   ( FeCr70C70Si2LP )
      FeCr70C70Si2LS   ( FeCr70C70Si2LS )
      FeCr70C70Si2LSLP   ( FeCr70C70Si2LSLP )
      FeCr70C70Si4   ( FeCr70C70Si4 )
      FeCr70C70Si4LP   ( FeCr70C70Si4LP )
      FeCr70C70Si4LS   ( FeCr70C70Si4LS )
      FeCr70C70Si4LSLP   ( FeCr70C70Si4LSLP )
      FeCr70C70Si6   ( FeCr70C70Si6 )
      FeCr70C70Si6LP   ( FeCr70C70Si6LP )
      FeCr70C90   ( FeCr70C90 )
      FeCr70C90LP   ( FeCr70C90LP )
      FeCr70C90LS   ( FeCr70C90LS )
      FeCr70C90LSLP   ( FeCr70C90LSLP )
      FeCr70C90Si2   ( FeCr70C90Si2 )
      FeCr70C90Si2LP   ( FeCr70C90Si2LP )
      FeCr70C90Si2LS   ( FeCr70C90Si2LS )
      FeCr70C90Si2LSLP   ( FeCr70C90Si2LSLP )
      FeCr70C90Si4   ( FeCr70C90Si4 )
      FeCr70C90Si4LP   ( FeCr70C90Si4LP )
      FeCr70C90Si4LS   ( FeCr70C90Si4LS )
      FeCr70C90Si4LSLP   ( FeCr70C90Si4LSLP )
      FeCr80C01   ( FeCr80C01 )
      FeCr80C03   ( FeCr80C03 )
      FeCr80C05   ( FeCr80C05 )
      FeCr90C01   ( FeCr90C01 )
      FeCr90C03   ( FeCr90C03 )
      FeCr90C05   ( FeCr90C05 )
      FKh001A   ( ФХ001А )
      FKh001B   ( ФХ001Б )
      FKh002A   ( ФХ002А )
      FKh002B   ( ФХ002Б )
      FKh003A   ( ФХ003А )
      FKh003B   ( ФХ003Б )
      FKh004A   ( ФХ004А )
      FKh004B   ( ФХ004Б )
      FKh005A   ( ФХ005А )
      FKh005B   ( ФХ005Б )
      FKh006A   ( ФХ006А )
      FKh006B   ( ФХ006Б )
      FKh010A   ( ФХ010А )
      FKh019B   ( ФХ010Б )
      FKh015A   ( ФХ015А )
      FKh015B   ( ФХ015Б )
      FKh025A   ( ФХ025А )
      FKh025B   ( ФХ025Б )
      FKh050A   ( ФХ050А )
      FKh050B   ( ФХ050Б )
      FKh100A   ( ФХ100А )
      FKh100B   ( ФХ100Б )
      FKh200A   ( ФХ200А )
      FKh200B   ( ФХ200Б )
      FKh400A   ( ФХ400А )
      FKh400B   ( ФХ400Б )
      FKh650A   ( ФХ650А )
      FKh650B   ( ФХ650Б )
      FKh800A   ( ФХ800А )
      FKh800B   ( ФХ800Б )
      FKh850A   ( ФХ850А )
      FKh850B   ( ФХ850Б )
      FKh900A   ( ФХ900А )
      FKh900B   ( ФХ900Б )
      FKhN100A   ( ФХН100А )
      FKhN100B   ( ФХН100Б )
      FKhN200A   ( ФХН200А )
      FKhN200B   ( ФХН200Б )
      FKhN400A   ( ФХН400А )
      FKhN400B   ( ФХН400Б )
      FKhN600A   ( ФХН600А )
      FKhN600B   ( ФХН600Б )
 
Ferro-alloys - all grades in Database of Steel and Alloy ( Marochnik)
T o p

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru