Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | FeNb60Ta1A13.5 ( FeNb60Ta1A13.5 ) |
Classification : | Ferroniobium |
Equivalent grades: | Is absent |
C | Si | S | P | Nb | Ti | Al | Sn | Ta |
max 0.15 | max 4 | max 0.05 | max 0.15 | 55 - 70 | max 2.5 | max 3.5 | max 0.1 | max 2 |
B12 - Ferroalloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |