Characteristics for grade     Mg95   ( Мг95 )



      Grade :     Mg95   ( Мг95 )
      Classification :   Primary magnesium
      Equivalent grades:   Go here



Chemical composition in % for grade   Mg95   ( Мг95 )
Fe Si Mn NiAl Cu Pb Mg Zn Sn Na Cl Impurity
max   0.003max   0.004max   0.01max   0.001max   0.01max   0.003max   0.005min   99.95max   0.01max   0.005max   0.004max   0.005other, each 0.01; all 0.05


Mechanical properties under Т=20oС for grade   Mg95   ( Мг95 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
casted     85-130  3-6   
deformed     250   8-10   


    Brinell hardness for     Mg95   ( Мг95 )   ,     casted HB 10 -1 = 30   MPa
    Brinell hardness for     Mg95   ( Мг95 )   ,     deformed HB 10 -1 = 50   MPa
    Brinell hardness for     Mg95   ( Мг95 )   ,     annealed HB 10 -1 = 40   MPa


Technological properties of the material   Mg95   ( Мг95 ) .
        Melting temperature : 651   °C


Physical properties for grade   Mg95   ( Мг95 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.45     1740   47
100   0.26        


Equivalent steels for grade     Mg95   ( Мг95 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyCanada
-DIN,WNrHG
9995A
H-99.95
99.95
99.97
99.99



Types of delivery of grade   Mg95   ( Мг95 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  Mg95   ( Мг95 ) - Primary magnesium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys