Magnesium - all grades


Primary magnesium
      Mg80   ( Мг80 )
      Mg90   ( Мг90 )
      Mg95   ( Мг95 )
      Mg96   ( Мг96 )
      Mg98   ( Мг98 )
 

The magnesium alloy for burdening
      MA10Ts1   ( МА10Ц1 )
      MA8Ts   ( МА8Ц )
      MA8TsBch   ( МА8ЦБч )
      MA8TsCh   ( МА8Цч )
      MA8TsEh   ( МА8Цэ )
      MM2   ( ММ2 )
      MM2Ch   ( ММ2ч )
      MTsR1N3   ( МЦр1Н3 )

Magnesium for casting
      ML10   ( МЛ10 )
      ML11   ( МЛ11 )
      ML12   ( МЛ12 )
      ML15   ( МЛ15 )
      ML19   ( МЛ19 )
      ML2   ( МЛ2 )
      ML3   ( МЛ3 )
      ML4   ( МЛ4 )
      ML4pch   ( МЛ4пч )
      ML5   ( МЛ5 )
      ML5on   ( МЛ5он )
      ML5pch   ( МЛ5пч )
      ML6   ( МЛ6 )
      ML8   ( МЛ8 )
      ML9   ( МЛ9 )
 

Wrought magnesium
      MА1   ( МА1 )
      MА11   ( МА11 )
      MА12   ( МА12 )
      MА14   ( МА14 )
      MА15   ( МА15 )
      MА17   ( МА17 )
      MА18   ( МА18 )
      MА19   ( МА19 )
      MА2   ( МА2 )
      Ma2-1   ( Ма2-1 )
      MA2-1PCh   ( МА2-1пч )
      MA20   ( МА20 )
      MА21   ( МА21 )
      MА5   ( МА5 )
      MА8   ( МА8 )
      MA8PCh   ( МА8пч )

Magnesium with specified properties
      MА2-2   ( МА2-2 )
      ML16   ( МЛ16 )
      ML16vch   ( МЛ16вч )
      ML16pch   ( МЛ16пч )
      ML4vch   ( МЛ4вч )
      MTSI   ( МЦИ )
Magnesium - all grades in Database of Steel and Alloy ( Marochnik)
T o p

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru