Characteristics for grade     ML19   ( МЛ19 )



      Grade :     ML19   ( МЛ19 )
      Classification :   Magnesium for casting
      Equivalent grades:     Is absent



Chemical composition in % for grade   ML19   ( МЛ19 )
Fe Si NiAl Cu Zr Be Mg Zn Nd Y Impurity
max   0.01max   0.03max   0.005max   0.03max   0.030.4 - 1max   0.00194.41 - 96.50.1 - 0.61.6 - 2.31.4 - 2.2other 0.14; all 0.25
Comment: Mg is a basis; the percentage of Mg is given approximately.


Mechanical properties under Т=20oС for grade   ML19   ( МЛ19 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 2856-79     220 120 3    


    Brinell hardness for     ML19   ( МЛ19 )   ,       HB 10 -1 = 28   MPa


Technological properties of the material   ML19   ( МЛ19 ) .
        Linear shrinkage : 1.2 - 1.5   %


Physical properties for grade   ML19   ( МЛ19 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.43   87.9 1790 1130.4  
100   27.7        



Types of delivery of grade   ML19   ( МЛ19 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  ML19   ( МЛ19 ) - Magnesium for casting: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys