Grade : | MА15 ( МА15 ) |
Classification : | Wrought magnesium |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ni | Al | Cu | Zr | Be | Mg | Zn | Cd | La | Impurity |
max 0.03 | max 0.05 | max 0.1 | max 0.005 | max 0.05 | max 0.03 | 0.45 - 0.9 | max 0.002 | 95.33 - 97.05 | 2.5 - 3.5 | 1.2 - 2 | 0.7 - 1.1 | all 0.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet annealed , GOST 22635-77 | 250-260 | 170-180 | 4-6 | |||||
Bar, GOST 18351-73 | 275-295 | 215-235 | 5-6 |
Brinell hardness for MА15 ( МА15 ) , | HB 10 -1 = 60 MPa |
Linear shrinkage : | 3.2 % |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.42 | 113 | 1830 | 65 | ||
100 | 25.9 | 1004.8 | ||||
200 | 26.8 | |||||
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B53 - Sheets and Strips |
B55 - Bars |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |