Characteristics for grade     MА2   ( МА2 )



      Grade :     MА2   ( МА2 )
      Classification :   Wrought magnesium
      Equivalent grades:   Go here



Chemical composition in % for grade   MА2   ( МА2 )
Fe Si Mn NiAl Cu Be Mg Zn Impurity
max   0.05max   0.10.15 - 0.5max   0.0053 - 4max   0.05max   0.00294.493 - 96.650.2 - 0.8 all 0.3
Comment: Mg is a basis; the percentage of Mg is given approximately.


Mechanical properties under Т=20oС for grade   MА2   ( МА2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 18351-73     215-245125 5-6   


    Brinell hardness for     MА2   ( МА2 )   ,       HB 10 -1 = 45   MPa


Technological properties of the material   MА2   ( МА2 ) .
        Linear shrinkage : 5   %


Physical properties for grade   MА2   ( МА2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.42   96.3 1780   120
100   26     1130.4  


Equivalent steels for grade     MА2   ( МА2 )
Warning! Indicated both exact and nearest equivalents.
USAJapanEngland
-JIS BS
AZ31B
AZ31C
MB1
MP1
MS1
MAG-E-111
MAG-S-111



Types of delivery of grade   MА2   ( МА2 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B52 - Graded and shaped rolling
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  MА2   ( МА2 ) - Wrought magnesium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru