Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | MA2-1PCh ( МА2-1пч ) |
Classification : | Wrought magnesium |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ni | Al | Cu | Be | Mg | Zn | Impurity |
max 0.005 | max 0.01 | 0.2 - 0.6 | max 0.001 | 3.8 - 5 | max 0.01 | max 0.002 | 92.872 - 95.2 | 0.8 - 1.5 | all 0.1 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet annealed , GOST 22635-77 | 260 | 150-160 | 8-10 | |||||
Pipe, GOST 19441-74 | 230 | 8 | ||||||
Bar, GOST 18351-73 | 245-255 | 145 | 5-8 | |||||
Plate , GOST 21990-76 | 230-250 | 140 | 6-8 |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1790 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B52 - Graded and shaped rolling |
B53 - Sheets and Strips |
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |