Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Magnesium

Characteristics for grade     MА21   ( МА21 )



      Grade :   MА21   ( МА21 ) (   ИМВ2   )
      Classification :   Wrought magnesium
      Equivalent grades:     Is absent



Chemical composition in % for grade   MА21   ( МА21 )
Fe Si Mn Ni CeAl Cu Mg Zn CdNa Li Impurity
max   0.03max   0.1max   0.1max   0.005max   0.154.3 - 5.3max   0.0476.5 - 85.11 - 24 - 5max   0.0057.5 - 9 all 0.3
Comment: Mg is a basis; the percentage of Mg is given approximately.


Mechanical properties under Т=20oС for grade   MА21   ( МА21 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
      240 190 18.5 2670 


    Brinell hardness for     MА21   ( МА21 )   ,       HB 10 -1 = 75   MPa


Physical properties for grade   MА21   ( МА21 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.46     1600    



Types of delivery of grade   MА21   ( МА21 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  MА21   ( МА21 ) - Wrought magnesium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru