Grade : | Sv-08Kh16N8M2 ( Св-08Х16Н8М2 ) ( ЭП-377 ) |
Classification : | Welding steel wire |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | Mo |
0.05 - 0.1 | max 0.6 | 1.5 - 2 | 7.5 - 9 | max 0.018 | max 0.025 | 15 - 17 | 1.5 - 2 |
В05 - Welding and cutting of metals., Soldering, riveting |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |