Materials for welding and soldering - all grades


Welding steel wire
      Sv-01Kh19N9   ( Св-01Х19Н9 )
      Sv-01Kh23N28M3D3T   ( Св-01Х23Н28М3Д3Т )
      Sv-04Kh19N11M3   ( Св-04Х19Н11М3 )
      Sv-04Kh19N9   ( Св-04Х19Н9 )
      Sv-04Kh19N9S2   ( Св-04Х19Н9С2 )
      Sv-04Kh2MA   ( Св-04Х2МА )
      Sv-05Kh19N9F3S2   ( Св-05Х19Н9Ф3С2 )
      Sv-05Kh20N9FBS   ( Св-05Х20Н9ФБС )
      Sv-06N3   ( Св-06Н3 )
      Sv-06Kh14   ( Св-06Х14 )
      Sv-06Kh15N60M15   ( Св-06Х15Н60М15 )
      Sv-06Kh19N10M3T   ( Св-06Х19Н10М3Т )
      Sv-06Kh19N9T   ( Св-06Х19Н9Т )
      Sv-06Kh20N11M3TB   ( Св-06Х20Н11М3ТБ )
      Sv-06Kh25N12TYu   ( Св-06Х25Н12ТЮ )
      Sv-07Kh18N9TYu   ( Св-07Х18Н9ТЮ )
      Sv-07Kh19N10B   ( Св-07Х19Н10Б )
      Sv-07Kh25N12G2T   ( Св-07Х25Н12Г2Т )
      Sv-07Kh25N13   ( Св-07Х25Н13 )
      Sv-08   ( Св-08 )
      Sv-08A   ( Св-08А )
      Sv-08AA   ( Св-08АА )
      Sv-08G2S   ( Св-08Г2С )
      Sv-08GA   ( Св-08ГА )
      Sv-08GS   ( Св-08ГС )
      Sv-08GSMT   ( Св-08ГСМТ )
      Sv-08MKh   ( Св-08МХ )
      Sv-08N50   ( Св-08Н50 )
      Sv-08Kh14GNT   ( Св-08Х14ГНТ )
      Sv-08Kh16N8M2   ( Св-08Х16Н8М2 )
      Sv-08Kh18N8G2B   ( Св-08Х18Н8Г2Б )
      Sv-08Kh19N10G2B   ( Св-08Х19Н10Г2Б )
      Sv-08Kh19N10M3B   ( Св-08Х19Н10М3Б )
      Sv-08Kh19N9F2S2   ( Св-08Х19Н9Ф2С2 )
      Sv-08Kh1DYu   ( Св-08Х1ДЮ )
      Sv-08Kh20N9G7T   ( Св-08Х20Н9Г7Т )
      Sv-08Kh21N10G6   ( Св-08Х21Н10Г6 )
      Sv-08Kh25N13BTYu   ( Св-08Х25Н13БТЮ )
      Sv-08Kh3G2SM   ( Св-08Х3Г2СМ )
      Sv-08KhG2S   ( Св-08ХГ2С )
      Sv-08KhGSMA   ( Св-08ХГСМА )
      Sv-08KhGSMFA   ( Св-08ХГСМФА )
      Sv-08KhM   ( Св-08ХМ )
      Sv-08KhMNFBA   ( Св-08ХМНФБА )
      Sv-08KhMFA   ( Св-08ХМФА )
      Sv-08KhN2G2SMYu   ( Св-08ХН2Г2СМЮ )
      Sv-08KhN2GMTA   ( Св-08ХН2ГМТА )
      Sv-08KhN2GMYu   ( Св-08ХН2ГМЮ )
      Sv-08KhN2M   ( Св-08ХН2М )
      Sv-08KhNM   ( Св-08ХНМ )
      Sv-09Kh16N25M6AF   ( Св-09Х16Н25М6АФ )
      Sv-10G2   ( Св-10Г2 )
      Sv-10G2SMA   ( Св-10Г2СМА )
      Sv-10GA   ( Св-10ГА )
      Sv-10GN   ( Св-10ГН )
      Sv-10GSMT   ( Св-10ГСМТ )
      Sv-10MKh   ( Св-10МХ )
      Sv-10NMA   ( Св-10НМА )
      Sv-10Kh11NVMF   ( Св-10Х11НВМФ )
      Sv-10Kh16N25AM6   ( Св-10Х16Н25АМ6 )
      Sv-10Kh17T   ( Св-10Х17Т )
      Sv-10Kh20N15   ( Св-10Х20Н15 )
      Sv-10Kh5M   ( Св-10Х5М )
      Sv-10KhG2SMA   ( Св-10ХГ2СМА )
      Sv-10KhM   ( Св-10ХМ )
      Sv-10KhMFA   ( Св-10ХМФА )
      Sv-10KhMFT   ( Св-10ХМФТ )
      Sv-10KhN2GMT   ( Св-10ХН2ГМТ )
      Sv-12GS   ( Св-12ГС )
      Sv-12Kh11NMF   ( Св-12Х11НМФ )
      Sv-12Kh13   ( Св-12Х13 )
      Sv-13Kh25N18   ( Св-13Х25Н18 )
      Sv-13Kh25T   ( Св-13Х25Т )
      Sv-13Kh2MFT   ( Св-13Х2МФТ )
      Sv-15GSTYuTsA   ( Св-15ГСТЮЦА )
      Sv-18KhGS   ( Св-18ХГС )
      Sv-18KhMA   ( Св-18ХМА )
      Sv-20GSTYuA   ( Св-20ГСТЮА )
      Sv-20Kh13   ( Св-20Х13 )
      Sv-30Kh15N35V3BT   ( Св-30Х15Н35В3Б3Т )
      Sv-30Kh25N16G7   ( Св-30Х25Н16Г7 )
 
Materials for welding and soldering - all grades in Database of Steel and Alloy ( Marochnik)
T o p

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru