Characteristics for grade     Sv-04Kh19N9S2   ( Св-04Х19Н9С2 )

      Grade :     Sv-04Kh19N9S2   ( Св-04Х19Н9С2 )
      Classification :   Welding steel wire
      Equivalent grades:     Is absent



Chemical composition in % for grade   Sv-04Kh19N9S2   ( Св-04Х19Н9С2 )
C Si Mn Ni S P Cr
max   0.062 - 2.751 - 28 - 10max   0.018max   0.02518 - 20

Types of delivery of grade   Sv-04Kh19N9S2   ( Св-04Х19Н9С2 )
В05 - Welding and cutting of metals., Soldering, riveting


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  Sv-04Kh19N9S2   ( Св-04Х19Н9С2 ) - Welding steel wire: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru