Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - China | Standard - GB 13296-91 | Grade - 1Cr18Ni12Mo2Ti |
08KH17N13M2T ( 08Х17Н13М2Т ) - Corrosion-resistant steel for general purposes 08KH17N13M2T ( 08Х17Н13М2Т ), |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В62 - Steel pipes and connecting parts to them |