Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   Austria. Casting steel    

Equivalents to grade GS21Mn5

    Country   -   Austria         Standard   -   ONORM         Grade   -   GS21Mn5    

    20GL   ( 20ГЛ )   -   Casting alloy steel for general purposes

  20GL   ( 20ГЛ ),      



20GL   ( 20ГЛ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 20GL   ( 20ГЛ )
B42 - Rails: Pads, Pads, Crutches
B82 - Steel Castings
B83 - Castings with special properties (cast iron and steel)


GS21Mn5 Austria Casting steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru