Equivalents to grade Z1NCDU31-27-03

    Country   -   France         Standard   -   AFNOR NF         Grade   -   Z1NCDU31-27-03    

    06KHN28MDT   ( 06ХН28МДТ )   -   Corrosion-resistant alloy

  06KHN28MDT   ( 06ХН28МДТ ),      

06KHN28MDT   ( 06ХН28МДТ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 06KHN28MDT   ( 06ХН28МДТ )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them


Z1NCDU31-27-03 France Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru