Equivalents to grade Vch15

    Country   -   Bulgaria         Standard   -   BDS         Grade   -   Vch15    

    SCH15   ( СЧ15 )   -   Grey cast iron

  SCH15   ( СЧ15 ),      

SCH15   ( СЧ15 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade SCH15   ( СЧ15 )
B11 - Cast Iron
В61 - Pipes of ferrous metals and alloys cast and connecting parts to them
В81 - Castings of cast iron (gray and malleable cast iron)


Vch15 Bulgaria Cast iron:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...