Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - England | Standard - BS | Grade - 304S11 |
08KH18N10 ( 08Х18Н10 ) - Corrosion-resistant high-temperature steel 03KH18N11 ( 03Х18Н11 ) - Corrosion-resistant steel for general purposes 04KH18N10 ( 04Х18Н10 ) - Corrosion-resistant steel for general purposes 08KH18N10 ( 08Х18Н10 ), 03KH18N11 ( 03Х18Н11 ), 04KH18N10 ( 04Х18Н10 ), |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B34 - Ribbons |
В62 - Steel pipes and connecting parts to them |
B73 - Steel Alloy Wire |
B76 - Metal nets |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В62 - Steel pipes and connecting parts to them |
© 2003 - 2024 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |